TYP | POzorność | OPORNOŚĆ ELEKTRYCZNA | PRZEWODNICTWO CIEPLNE (100°C) | WSPÓŁCZYNNIK ROZSZERZENIA RMALE (TEMPERATURA POKOJOWA-600°C) | TWARDOŚĆ Shore'a | WYTRZYMAŁOŚĆ GIĘCIA | WYTRZYMAŁOŚĆ NA ŚCISKANIE | MODUŁ ELASTYCZNOŚCI | POROWATOŚĆ | POPIÓŁ | OCZYŚĆ POPIÓŁ | ROZMIAR CZĄSTEK |
G/cm3 | ΜΩm | W/mk | 10-6/°C | HSD | MPa | MPa | GP | % | PPM | PPM | Mikron | |
VET-4 | 1,75 | 8-11 | 121.1 | 5,46 | 42 | 38 | 65 | 9 | 17 | 500 | 50 | 13-15 |
VET-5 | 1,85 | 8-10 | 139,2 | 4,75 | 48 | 46 | 85 | 11.8 | 13 | 500 | 50 | 13-15 |
VET-5S | 1,68 | 13 | 90 | 5 | 51 | 38 | 86 | 8.8 | 18 | 500 | 50 | 13-15 |
VET-6 | 1.9 | 8-9 | 140 | 5.1 | 53 | 55 | 95 | 12 | 11 | / | 50 | 8-10 |
VET-7 | 1,82 | 11-13 | 85 | 5.6 | 65 | 51 | 115 | 11 | 12 | 500 | 50 | 8-10 |
VET-8 | 1,91 | 11-13 | 85 | 5,85 | 70 | 60 | 135 | 12 | 11 | 500 | 50 | 8-10 |