Ua lilo nā mea hana kalapona/carbon composite i hanauna hou o nā mea hoʻoheheʻe e hoʻololi i nā mea metala i hoʻokumu ʻia ma muli o ko lākou ʻano mechanical, thermal a friction a ʻaʻahu.
ʻO kāna mau hiʻohiʻona nui e like me kēia:
(1) ʻO ka haʻahaʻa o ka mea haʻahaʻa e like me 1.5g/cm3, hiki ke hōʻemi nui i ka nui o ka hana o ka disc brake;
(2) He kūʻē maikaʻi loa ka waiwai a he lōʻihi ke ola o ka disc brake, ʻoi aku ia ma mua o ʻelua mau mea o nā mea metala matrix composite;
(3) Paʻa dynamic friction kumu, maikaʻi anti-sticking a me anti-adhesion waiwai;
(4) E hoʻomaʻamaʻa i ka hoʻolālā disc brake a ʻaʻole koi i nā lining friction hou aku, nā mea hoʻohui, nā iwi kīwaha, a pēlā aku;
(5) Li'ili'i ka ho'onui wela, ka wela kiko'ī ki'eki'e ('elua o ka hao), a me ke ki'eki'e o ka wela;
(6) He kiʻekiʻe ka wela hana a me ka pale wela a hiki i 2700 ℃.
ʻIkepili ʻenehana o Carbon-Huina Kalapona | ||
Papa kuhikuhi | Unite | Waiwai |
ʻAno nui | g/cm3 | 1.40-1.50 |
ʻAno kalapona | % | ≥98.5~99.9 |
Lehu | PPM | ≤65 |
Ka hoʻoili wela (1150 ℃) | W/mk | 10~30 |
Ka ikaika tensile | Mpa | 90~130 |
Ikaika Flexural | Mpa | 100~150 |
Ka ikaika compressive | Mpa | 130~170 |
Ka ikaika shear | Mpa | 50~60 |
Interlaminar Shear ikaika | Mpa | ≥13 |
ʻAiʻa uila | Ω.mm2/m | 30~43 |
Coefficient o ka hoonui wela | 106/K | 0.3-1.2 |
Hoʻoponopono Mahana | ℃ | ≥2400 ℃ |
ʻO ka maikaʻi o ka pūʻali koa, ka hoʻoheheʻe ʻana i ka umu hoʻoheheʻe kemika piha, lawe ʻia mai ka Toray carbon fiber T700 i ulana mua ʻia 3D wili nila. Nā kikoʻī kikoʻī: ʻoi aku ka nui o ke anawaena o waho 2000mm, ka mānoanoa o ka paia 8-25mm, ke kiʻekiʻe 1600mm |