Volumen Densitas (g/cm3): 0.22-0.28
Tensile Fortitudo (Mpa): 2.5 (Deformation 5%)
Scelerisque Conductivity (W/mk): 0.15-0.25(25) 0.40-0.45(1400)
Imprimis Resistentia (Ohm.cm): 0.18-0.22
Carbon Content (%): ≥99
Cineres Content (%): ≤0.6
Absorptio humoris (%): ≤1.6
Purificationis Scala: Hight Puritas
Processing Temperature : 1450-2000
Praesto Location:
Plate: 1500* 1800(Max) Crassitudo 20-200mm
Circum Drum: 1500*2000(Max) Thicknes 20-150mm
Quadratus Drum: 1500*1500*2000(Max) Crassitudo 60-120mm
Applicative Temperature Range : 1250-2600
Agri applicationes:
• Vacuum fornacibus
• Inert gas fornacibus
• æstus curatio
obduratio, carbonisatio, brazing, etc.
• Carbon fibra productio
• Ferreus metallum productio
• Sintering applications
•Technica tellus productio
•CVD/PVD coasting
| |||||||||||||||||||||||||
|