Advantage :
1.CO2 Reactivity Residue can reach above 91%, Air Reactivity can reach above 96%;the life-span in cells of aluminium electrolysis is 30-33days.
2.Higher thermal shock Resistance
Thermal Exposure : <4*10
Heat Conductive : <3W/mkl
3.higher current density
current density : > 0.8A/cm2
4.lower Electrical Resistivity
Electrical Resistivity : 55-56μΩm
ANODE SPECIFICATION
Series
|
PROPERTY |
Unit |
Standard method |
Range |
1 |
Real Density |
g/cm3 |
ISO 8004 |
2 Min |
2 |
Apparent Density |
g/cm3 |
ISO 12985 |
1.52-1.58 |
3 |
Air permeability |
npm |
ISO 15906 |
0.5-1.5 |
5 |
Compressive Strength |
N/mm2 |
ISO 18515 |
40-48 |
6 |
Youngs moudle |
Gpa |
ISO 12989 |
4-5.5 |
7 |
Flexural Strength |
N/mm2 |
ISO 12986 |
8 – 10 |
8 |
Spe. Elec. Resistance |
µΩm |
ISO 11713 |
55-62 |
9 |
Cof. Lin . Thermal |
µm/(k.m) |
ISO 14420 |
3.75-4.5 |
10 |
Thermal Conductivity |
W/(k.m) |
ISO 129087 |
3-4.5 |
11 |
ASh |
% |
ISO 8005 |
0.5 Max |
12 |
Air Reactivity residue dust Lost
|
% % %
|
ISO 12989-1
|
75 – 85 4 – 8 10 – 20 |
13 |
Co2 Reactivity residue dust lost |
% % % |
ISO 12988-1
|
84 – 95 3 – 8 6 – 14 |
14 |
Elements S V Fe F Ca Al Ni SI |
% ppm // // // // // |
ASTM D6376
|
0.5 – 2.5 30 – 320 100 – 600 150 – 600 50 – 200 150 – 600 40 – 200 50 – 300 |